Electrical Properties Metric English Comments
Hot Wire Ignition, HWI 4.0 sec
4.0 sec
Eurostar Staramide RF00ASXP PA66, 50% Glass Filled, Injection Molded
Staramide RF00ASXP is a 50% Glass Fiber Reinforced Polyamide 66 Injection Molding Resin (also known as Staramide 66 G 50V S3)Information provided by Eurostar.
Copyright © lookpolymers.com All Rights Reserved