Electrical Properties | Metric | English | Comments |
---|---|---|---|
Hot Wire Ignition, HWI | 33.4 sec | 33.4 sec | UL746A |
Shuman 790 Black and Custom Colors ABS-Flame Retardant Excellent flame retardancy, good impact strength, good chemical resistance, good wear and abrasion resistance.Data provided by the manufacturer. |
|||
Hot Wire Ignition, HWI | 33.4 sec | 33.4 sec | UL746A |
Shuman 791 Black and Custom Colors ABS-Flame Retardant Long term thermal aging rated. Excellent flame retardancy, good impact strength, good chemical resistance, good wear and abrasion resistance.Data provided by the manufacturer. |