Electrical Properties | Metric | English | Comments |
---|---|---|---|
Curie Temperature | 700 °C | 1290 °F | |
Ceradyne SEMICORE® S1-5A MMOA 20/15 SmCo5 Samarium Cobalt Magnet Magnetic alignment at 90° to Compaction AxisApplications:Microwave amplifiers and oscillators for airborne equipmentTWT modules for phased array radarSmall motors for severe thermal conditions Herm.. |
|||
Curie Temperature | 700 °C | 1290 °F | |
Ceradyne SEMICORE® S1-5B MMPA 16/18 SmCo5 Samarium Cobalt Magnet Magnetic alignment parallel to Compaction AxisApplications:Microwave amplifiers and oscillators for airborne equipmentTWT modules for phased array radarSmall motors for severe thermal conditions Her.. |
|||
Curie Temperature | 700 °C | 1290 °F | |
Ceradyne SEMICORE® S1-5C Specials SmCo5 Samarium Cobalt Magnet Applications:Microwave amplifiers and oscillators for airborne equipmentTWT modules for phased array radarSmall motors for severe thermal conditions Hermetic magnetic couplings to replace shaft seal.. |