Electrical Properties | Metric | English | Comments |
---|---|---|---|
Curie Temperature | 310 °C | 590 °F | |
Alliance N-35 Neodymium Iron Boron Magnetic Material |
|||
Curie Temperature | 310 °C | 590 °F | |
Alliance N-38 Neodymium Iron Boron Magnetic Material |
|||
Curie Temperature | 310 °C | 590 °F | |
Alliance N-42 Neodymium Iron Boron Magnetic Material |
|||
Curie Temperature | 310 °C | 590 °F | |
Alliance N-45 Neodymium Iron Boron Magnetic Material |
|||
Curie Temperature | 310 °C | 590 °F | |
Alliance N-50 Neodymium Iron Boron Magnetic Material |
|||
Curie Temperature | 310 °C | 590 °F | |
Alliance N-33 Neodymium Iron Boron Magnetic Material |
|||
Curie Temperature | 310 °C | 590 °F | |
Alliance N-40 Neodymium Iron Boron Magnetic Material |
|||
Curie Temperature | 310 °C | 590 °F | |