Electrical Properties | Metric | English | Comments |
---|---|---|---|
Curie Temperature | 435 °C | 815 °F | |
Carpenter Kovar® Alloy (Glass and Ceramic Sealing Alloy) Data provided by Carpenter Technology Corporation.Kovar® alloy is a vacuum melted, Fe-Ni-Co, low expansion alloy whose chemical composition is controlled within narrow limits to assure precise unif.. |