Electrical Properties | Metric | English | Comments |
---|---|---|---|
Curie Temperature | 380 °C | 716 °F | |
Goodfellow Nickel Base Magnetic Shielding Alloy - Mu Metal High Nickel magnetically soft alloy used for magnetic shielding, high quality but low noise audio frequency transformers, ground fault interrupter cores, anti-shoplifting devices, tape recorder head.. |