Electrical Properties | Metric | English | Comments |
---|---|---|---|
Curie Temperature | 150 °C | 302 °F | |
PPT FP150 Fully Sintered Ferrite Powder Fully sintered NiZn ferrite, MnZn ferrite, and MgZn ferrite powders are available. Spherical or irregular particle shapes in custom particle sizes are available, ranging from sub-micron to a few hu.. |
|||
Curie Temperature | 150 °C | 302 °F | |
PPT LSF180 Low Sintering Temperature Ferrite Powder Uses: Low Temperature Co-fired Ceramic Components (LTCC), Multi-Layer Chip Inductors (MLCI), Chip Beads (EMI Suppressors)Electromagnetic proerties reported were tested on sintered toroids with a HP4.. |
|||
Curie Temperature | 150 °C | 302 °F | |
PPT LSF220 Low Sintering Temperature Ferrite Powder Uses: Low Temperature Co-fired Ceramic Components (LTCC), Multi-Layer Chip Inductors (MLCI), Chip Beads (EMI Suppressors)Electromagnetic proerties reported were tested on sintered toroids with a HP4.. |
|||
Curie Temperature | 150 °C | 302 °F | |
PPT LSF400 Low Sintering Temperature Ferrite Powder Uses: Low Temperature Co-fired Ceramic Components (LTCC), Multi-Layer Chip Inductors (MLCI), Chip Beads (EMI Suppressors)Electromagnetic proerties reported were tested on sintered toroids with a HP4.. |
|||
Curie Temperature | 150 °C | 302 °F | |
Piezo Kinetics 906 Lead Nickel Niobate Piezoelectric PKI 906 is slightly different in composition than the "general" PZT formulations. Its PZT-doped Lead Nickel Niobate composition was developed to enhance the d33 and dielectric properties of Navy Typ.. |
|||
Curie Temperature | 150 °C | 302 °F | |
PPT BP780 NiZn Ferrite Powder Uses: EMI Suppressors, Wave Absorbing Tiles, Impeders, Multi-Hole Connectors, Inductors, Transformers, Converters, Choke Coils, AntennasElectromagnetic characteristics were tested on toroid with a H.. |