Electrical Properties | Metric | English | Comments |
---|---|---|---|
Curie Temperature | 190 °C | 374 °F | |
Special Metals NI-SPAN-C® Alloy 902 A nickel-iron-chromium alloy made precipitation hardenable by additions of aluminum and titanium. The titanium content also helps provide a controllable thermoelastic coefficient, which is the allo.. |
|||
Curie Temperature | >= 190 °C | >= 374 °F | |
Channel Industries 5700 Lead Zirconate Titanate Piezoelectric Navy Type VICharacterized by high coupling factors and high piezoelectric and dielectric constants over extended temperature ranges and stress amplitudes, lead zirconate titanates are the most exten.. |