Polymer Property : Curie Temperature = 160 °C Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Curie Temperature 160 °C
320 °F
PPT BP860 NiZn Ferrite Powder
Uses: EMI Suppressors, Wave Absorbing Tiles, Impeders, Multi-Hole Connectors, Inductors, Transformers, Converters, Choke Coils, AntennasElectromagnetic characteristics were tested on toroid with a H..
Curie Temperature 160 °C
320 °F
PPT FP160 Fully Sintered Ferrite Powder
Fully sintered NiZn ferrite, MnZn ferrite, and MgZn ferrite powders are available. Spherical or irregular particle shapes in custom particle sizes are available, ranging from sub-micron to a few hu..
Curie Temperature 160 °C
320 °F
PPT BP600 NiZn Ferrite Powder
Uses: EMI Suppressors, Wave Absorbing Tiles, Impeders, Multi-Hole Connectors, Inductors, Transformers, Converters, Choke Coils, AntennasElectromagnetic characteristics were tested on toroid with a H..