Polymer Property : Curie Temperature = -124.4 °C Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Curie Temperature -124.4 °C
-191.9 °F
Carlson C 600 Nickel-Chromium-Iron Alloy
Carlson Alloy C 600 is nickel-chromium alloy, developed for use in severely corrosive environments at elevated temperatures. The high nickel content of this alloy provides excellent resistance to c..
Curie Temperature -124.4 °C
-191.9 °F
Carlson C 600ESR Nickel-Chromium-Iron Alloy
General DescriptionCarlson Alloy C 600 is nickel-chromium alloy, developed for use in severely corrosive environments at elevated temperatures. The high nickel content of this alloy provides excell..