Electrical Properties | Metric | English | Comments |
---|---|---|---|
Magnetic Remanence, Br | 8400 Gauss | 8400 Gauss | 1850°F, 4 hours, Dry Hydrogen |
ATI Allegheny Ludlum Relay Steels No. 5 Silicon and iron alloyApplications:relays, armatures, solenoids, magnetic clutches, pole pieces, certain types of motors, transformers, data processing equipment.Information provided by Allegheny Lu.. |