Electrical Properties | Metric | English | Comments |
---|---|---|---|
Magnetic Remanence, Br | 8000 Gauss | 8000 Gauss | |
PSM Industries PolyAlloys MIM-2200 Soft Magnetic Steel PolyAlloys Injected Metals, a division of PSM Industries, Inc., offers precision, High-Performance components for structural, magnetic and electronic applications that require a high degree of compl.. |
|||
Magnetic Remanence, Br | 8000 Gauss | 8000 Gauss | |
Alliance A-8S Alnico Magnetic Material |
|||
Magnetic Remanence, Br | 8000 - 8500 Gauss | 8000 - 8500 Gauss | |
Ceradyne SEMICORE® S1-5B MMPA 16/18 SmCo5 Samarium Cobalt Magnet Magnetic alignment parallel to Compaction AxisApplications:Microwave amplifiers and oscillators for airborne equipmentTWT modules for phased array radarSmall motors for severe thermal conditions Her.. |
|||
Magnetic Remanence, Br | 8000 - 9000 Gauss | 8000 - 9000 Gauss | |
Ceradyne SEMICORE® S2-17C Specials Sm2 (CoFeCuZr)17 Samarium Cobalt Magnet Applications:Microwave amplifiers and oscillators for airborne equipmentTWT modules for phased array radarSmall motors for severe thermal conditions Hermetic magnetic couplings to replace shaft seal.. |
|||
Magnetic Remanence, Br | 8000 Gauss | 8000 Gauss | |
Alliance A-8 Alnico Magnetic Material |