Polymer Property : Magnetic Remanence, Br = 14200 Gauss Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Magnetic Remanence, Br 14200 Gauss
14200 Gauss
Alliance N-50 Neodymium Iron Boron Magnetic Material