Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Magnetic Remanence, Br = 13500 Gauss Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Magnetic Remanence, Br 13500 Gauss
13500 Gauss
Alliance N-45 Neodymium Iron Boron Magnetic Material
Magnetic Remanence, Br 13500 Gauss
13500 Gauss
Alliance N-45M Neodymium Iron Boron Magnetic Material
Copyright © lookpolymers.com All Rights Reserved