Polymer Property : Magnetic Remanence, Br = 13300 Gauss Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Magnetic Remanence, Br 13300 Gauss
13300 Gauss
Alliance N-44H Neodymium Iron Boron Magnetic Material