Magnetic Remanence, Br 11900 Gauss
11900 Gauss
Alliance N-35 Neodymium Iron Boron Magnetic Material
Magnetic Remanence, Br 11900 Gauss
11900 Gauss
Alliance N-35H Neodymium Iron Boron Magnetic Material
Magnetic Remanence, Br 11900 Gauss
11900 Gauss
Alliance N-35M Neodymium Iron Boron Magnetic Material
Magnetic Remanence, Br 11900 Gauss
11900 Gauss
Alliance N-35SH Neodymium Iron Boron Magnetic Material
Magnetic Remanence, Br 11900 Gauss
11900 Gauss
Alliance N-35UH Neodymium Iron Boron Magnetic Material