Electrical Properties | Metric | English | Comments |
---|---|---|---|
Magnetic Remanence, Br | 10900 Gauss | 10900 Gauss | |
Alliance S-28A Samarium Cobalt Magnetic Material |
|||
Magnetic Remanence, Br | 10900 Gauss | 10900 Gauss | |
Alliance S-28B Samarium Cobalt Magnetic Material |
|||
Magnetic Remanence, Br | 10900 Gauss | 10900 Gauss | |
Alliance S-28H Samarium Cobalt Magnetic Material |