Electrical Properties | Metric | English | Comments |
---|---|---|---|
Magnetic Remanence, Br | 0.82 Gauss | 0.82 Gauss | Remanence Ratio, B<sub>r</sub>/B<sub>s</sub> |
Goodfellow Cobalt/Silicon/Boron/Iron/Nickel Alloy Metallic glasses (glassy alloys) or amorphous metals. Uses include soft magnetic applications, brazing, coating and as reinforcing fibers.Information provided by Goodfellow. |