Electrical Properties | Metric | English | Comments |
---|---|---|---|
Magnetic Remanence, Br | 0.68 Gauss | 0.68 Gauss | Remanence Ratio, B<sub>r</sub>/B<sub>s</sub> |
Goodfellow Iron 40/Nickel 38/Boron 18 Alloy Metallic glass (glassy alloy) or amorphous metal. Uses include soft magnetic applications, brazing, coating and as reinforcing fibers.Information provided by Goodfellow. |