Electrical Properties Metric English Comments
Magnetic Coercive Force, Hc 9600 Oe
9600 Oe
Alliance N-28UH Neodymium Iron Boron Magnetic Material
Magnetic Coercive Force, Hc 9600 Oe
9600 Oe
Intrinsic
Alliance BCN-14 Bonded (Composite) Magnetic Material