Electrical Properties | Metric | English | Comments |
---|---|---|---|
Magnetic Coercive Force, Hc | 30000 Oe | 30000 Oe | Intrinsic |
Alliance N-28EH Neodymium Iron Boron Magnetic Material |
|||
Magnetic Coercive Force, Hc | 30000 Oe | 30000 Oe | Intrinsic |
Alliance N-30EH Neodymium Iron Boron Magnetic Material |