Polymer Property : Magnetic Coercive Force, Hc = 2500 Oe Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Magnetic Coercive Force, Hc 2500 Oe
2500 Oe
Intrinsic
Alliance C-5 Strontium Ferrite Ceramic Magnetic Material