Electrical Properties | Metric | English | Comments |
---|---|---|---|
Magnetic Coercive Force, Hc | 2400 Oe | 2400 Oe | |
Alliance BIF-17 Bonded (Composite) Magnetic Material |
|||
Magnetic Coercive Force, Hc | 2400 Oe | 2400 Oe | |
Alliance C-5 Strontium Ferrite Ceramic Magnetic Material |