Polymer Property : Magnetic Coercive Force, Hc = 2.5 Oe Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Magnetic Coercive Force, Hc 1.25 - 2.5 Oe
1.25 - 2.5 Oe
Schmolz + Bickenbach IMRE™ Stainless Steel Bar
Description: Ugine IMRE™ is a chromium stainless steel with improved magnetic properties used in solenoid valves. IMRE™ is at 18% chromium ferritic stainless steel with 2% Mo designed to withstand..