Magnetic Coercive Force, Hc 17000 Oe
17000 Oe
Intrinsic
Alliance N-35H Neodymium Iron Boron Magnetic Material
Magnetic Coercive Force, Hc 17000 Oe
17000 Oe
Intrinsic
Alliance N-40H Neodymium Iron Boron Magnetic Material
Magnetic Coercive Force, Hc 17000 Oe
17000 Oe
Intrinsic
Alliance N-44H Neodymium Iron Boron Magnetic Material
Magnetic Coercive Force, Hc 17000 Oe
17000 Oe
Intrinsic
Alliance N-33H Neodymium Iron Boron Magnetic Material
Magnetic Coercive Force, Hc 17000 Oe
17000 Oe
Intrinsic
Alliance N-38H Neodymium Iron Boron Magnetic Material
Magnetic Coercive Force, Hc 17000 Oe
17000 Oe
Intrinsic
Alliance N-42H Neodymium Iron Boron Magnetic Material