Polymer Property : Magnetic Coercive Force, Hc = 14000 Oe Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Magnetic Coercive Force, Hc 14000 Oe
14000 Oe
Intrinsic
Alliance N-35M Neodymium Iron Boron Magnetic Material
Magnetic Coercive Force, Hc 14000 Oe
14000 Oe
Intrinsic
Alliance N-40M Neodymium Iron Boron Magnetic Material
Magnetic Coercive Force, Hc 14000 Oe
14000 Oe
Intrinsic
Alliance N-42M Neodymium Iron Boron Magnetic Material
Magnetic Coercive Force, Hc 14000 Oe
14000 Oe
Intrinsic
Alliance N-45M Neodymium Iron Boron Magnetic Material
Magnetic Coercive Force, Hc 14000 Oe
14000 Oe
Intrinsic
Alliance N-38M Neodymium Iron Boron Magnetic Material
Magnetic Coercive Force, Hc 14000 Oe
14000 Oe
Intrinsic
Alliance N-33M Neodymium Iron Boron Magnetic Material