Electrical Properties | Metric | English | Comments |
---|---|---|---|
Magnetic Coercive Force, Hc | 11600 Oe | 11600 Oe | |
Alliance N-40H Neodymium Iron Boron Magnetic Material |
|||
Magnetic Coercive Force, Hc | 11600 Oe | 11600 Oe | |
Alliance N-40M Neodymium Iron Boron Magnetic Material |
|||
Magnetic Coercive Force, Hc | 11600 Oe | 11600 Oe | |
Alliance N-42 Neodymium Iron Boron Magnetic Material |
|||
Magnetic Coercive Force, Hc | 11600 Oe | 11600 Oe | |
Alliance N-42M Neodymium Iron Boron Magnetic Material |
|||
Magnetic Coercive Force, Hc | 11600 Oe | 11600 Oe | |
Alliance N-40 Neodymium Iron Boron Magnetic Material |