Electrical Properties Metric English Comments
Magnetic Coercive Force, Hc 11300 Oe
11300 Oe
Alliance N-38 Neodymium Iron Boron Magnetic Material
Magnetic Coercive Force, Hc 11300 Oe
11300 Oe
Alliance N-38H Neodymium Iron Boron Magnetic Material
Magnetic Coercive Force, Hc 11300 Oe
11300 Oe
Alliance N-38M Neodymium Iron Boron Magnetic Material