Polymer Property : Magnetic Coercive Force, Hc = 10000 Oe Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Magnetic Coercive Force, Hc 10000 Oe
10000 Oe
Alliance S-28A Samarium Cobalt Magnetic Material
Magnetic Coercive Force, Hc 10000 Oe
10000 Oe
Alliance S-28B Samarium Cobalt Magnetic Material
Magnetic Coercive Force, Hc 10000 Oe
10000 Oe
Alliance S-28H Samarium Cobalt Magnetic Material
Magnetic Coercive Force, Hc 10000 Oe
10000 Oe
Alliance S-32 Samarium Cobalt Magnetic Material