Electrical Properties | Metric | English | Comments |
---|---|---|---|
Magnetic Coercive Force, Hc | 1.0 Oe | 1.0 Oe | |
PSM Industries PolyAlloys MIM-Fe-%3Si Grade 2 Soft Magnetic Steel PolyAlloys Injected Metals, a division of PSM Industries, Inc., offers precision, High-Performance components for structural, magnetic and electronic applications that require a high degree of compl.. |