Electrical Properties | Metric | English | Comments |
---|---|---|---|
Magnetic Coercive Force, Hc | 0.0126 Oe | 0.0126 Oe | |
Goodfellow Nickel Base Magnetic Shielding Alloy - Mu Metal High Nickel magnetically soft alloy used for magnetic shielding, high quality but low noise audio frequency transformers, ground fault interrupter cores, anti-shoplifting devices, tape recorder head.. |
|||
Magnetic Coercive Force, Hc | 0.0126 Oe | 0.0126 Oe | |
Goodfellow Nickel/Iron/Silicon/Boron Alloy Metallic glass (glassy alloy) or amorphous metal. Uses include soft magnetic applications, brazing, coating and as reinforcing fibers.Information provided by Goodfellow.Composition Notes: Si + B co.. |