Electrical Properties | Metric | English | Comments |
---|---|---|---|
Exciting Power | 297.27 VA/lb @Magnetic Field 1.70 T, Frequency 200 Hz |
297.27 VA/lb @Magnetic Field 1.70 T, Frequency 200 Hz |
ASTM A343, ASTM A348, 50/50, Stress Relief Annealed |
AK Steel DI-MAX® HF-10 Nonoriented Electrical Steel DI-MAX HF-10 is a fully processed nonoriented electrical steel designed for use in high speed motors, traction motors, aircraft generators, and other rotating equipment operating at frequencies abov.. |