Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Breakdown | 8800 V | 8800 V | ASTM D149 |
DuPont Teijin Films Melinex® 329 Polyester Film, 200 Gauge Melinex® 329 is an opaque white, non-pretreated, polyester film with good handling properties and a unique glossy appearance. It is used as a base for pressure sensitive labels, in security and ac.. |