Electrical Properties Metric English Comments
Dielectric Breakdown 7600 V
7600 V
3M 92015 Double Coated Tape with Adhesive 200MP
3M™ Double Coated Tapes with 3M™ Adhesive 200MP feature a thin polyester film for dimensional stability and improved handling with ease of die-cutting and laminating. The 3M adhesive 200MP provide..