Electrical Properties Metric English Comments
Dielectric Breakdown >= 6250 V

@Thickness 0.250 mm
>= 6250 V

@Thickness 0.00984 in
DIN EN 60243
CeramTec Rubalit® HSS Alumina, 75% (High Strength Substrate)
Rubalit® HSS (High Strength Substrate) displays the successful union of elasticity and strength. The ultrafine microstructure of Rubalit® HSS is the basis for its outstanding substrate surface qua..