Electrical Properties Metric English Comments
Dielectric Breakdown 5500 V
5500 V
1/4" electrode 500 V/sec 25°C in air; ASTM D149
DuPont Teijin Films Mylar® EL Polyester Film, 142 Gauge
Mylar® EL films, typically 48 through 500 gauge are strong, tough, general -purpose films for electrical/electronic uses. Heavier gauges of Mylar® EL films are similar to Mylar® MO films. Availab..
Dielectric Breakdown 5500 V
5500 V
1/4" electrode 500 V/sec 25°C in air; ASTM D149
DuPont Teijin Films Mylar® WC11/WC22 Polyester Film, 284 Gauge
Mylar® type WC11 films are general-purpose electrical grade films, similar to Mylar® EL. These clear to hazy films are tough and durable as a core wrap. They offer good dielectric and good handlin..
Dielectric Breakdown 5500 V
5500 V
1/4" electrode 500 V/sec 25°C in air; ASTM D149
DuPont Teijin Films Mylar® WC Polyester Film, 142 Gauge
Mylar® WC films are general-purpose electrical grade films, similar to Mylar® EL. These clear to hazy films are tough and durable as a core wrap. They offer good dielectrics and good handling char..
Dielectric Breakdown 5500 V
5500 V
1/4" electrode 500 V/sec 25°C in air; ASTM D149
DuPont Teijin Films Mylar® WC11/WC22 Polyester Film, 142 Gauge
Mylar® type WC11 films are general-purpose electrical grade films, similar to Mylar® EL. These clear to hazy films are tough and durable as a core wrap. They offer good dielectric and good handlin..