Dielectric Breakdown 47000 V
47000 V
Disc Electrodes at 60 hertz
ConocoPhillips Transformer Oil
Description: Conoco Transformer Oil, an insulating oil of very high dielectric strength, is suited for oil-filled transformers in both large substations and small pole-mounted transformers. It is al..