Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Breakdown | >= 4200 V | >= 4200 V | Withstand Voltage AC V |
Fujipoly Industries FLAT-5TV-10-.75 silicone rubber fusible tape Information provided by Fujipoly Industries |
|||
Dielectric Breakdown | >= 4200 V | >= 4200 V | Withstand Voltage AC V |
Fujipoly Industries FLAT-5TV-10-1.0 silicone rubber fusible tape Information provided by Fujipoly Industries |