Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Breakdown | 36110 V @Thickness 2.54 mm |
36110 V @Thickness 0.100 in |
ASTM D1816-04 |
Paratherm Corporation Paratherm™ CR Heat Transfer Fluid Paratherm CR® heat transfer fluid is a blend of synthetic components formulated to provide superior cooling performance in closed-loop heat-transfer systems operating down to -88°C (-127°F) yet i.. |