Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Breakdown | >= 22000 V | >= 22000 V | IEC 626 |
Dr. D. Mueller Flexiso® DMD FI 14010 00460 Polyester Electrical Insulation Structure: Flexiso® DMD, FI 14010 00460 is a flexible three layer material, consisting of a layer of polyester film, of which both sides have a layer of polyester fleece fabric and is coated with .. |