Electrical Properties Metric English Comments
Dielectric Breakdown 16000 V
16000 V
Saint-Gobain CHR® 2285-5 Extruded PTFE Film Backing Silicone Adhesive Pressure Sensitive Tape
Description: PTFE films provide a conformable release surface and exhibit a remarkably low coefficient of friction and non-stick properties. PTFE films have high temperature resistance and are virtu..
Dielectric Breakdown 16000 V

@Thickness 1.00 mm
16000 V

@Thickness 0.0394 in
CeramTec Alunit® Aluminum Nitride
Alunit® offers an extremely high thermal conductivity of 180 W/mK and outstanding electrical insulation properties. The thermal expansion coefficient of this material is comparable to silicon. Its ..
Dielectric Breakdown >= 16000 V

@Thickness 1.00 mm
>= 16000 V

@Thickness 0.0394 in
ASTM-D149
CeramTec Alunit® HS Aluminum Nitride
Alunit® HS offers an extremely high thermal conductivity of 170 W/mK and outstanding electrical insulation properties. The thermal expansion coefficient of this material is comparable to silicon. I..
Dielectric Breakdown 16000 V
16000 V
0.25 inch electrodes in dry air @25°C; ASTM D149-81
DuPont Teijin Films Melinex® S Polyester Film, 500 Gauge
Melinex® S is a general purpose film which combines excellent handling characteristics with a slightly hazy appearance. It is available in specific thicknesses from 48 - 500 gauge, and is used for ..
Dielectric Breakdown 16000 V

@Thickness 1.00 mm
16000 V

@Thickness 0.0394 in
ASTM-D149
CeramTec CeramCool® Alunit® Aluminum Nitride
CeramCool® is a metallized ceramic heat-sink for high power applications demonstrated by high power LED-systems. CeramCool® material characteristics: electrical insulation, high volume resistivit..