Electrical Properties Metric English Comments
Dielectric Breakdown 14000 V
14000 V
Withstand Voltage [V/min]; JIS-K-6249; ASTM D-149
Fujipoly Industries Sarcon® GR-c Gap Filler Pad
Sarcon GR-c is a highly conformable, thermally conductive (no electric conductive) and electromagnetic wave absorption material in areas where space between surfaces is uneven and surface textures v..
Dielectric Breakdown 14000 V
14000 V
Withstand Voltage [V/min]; JIS-K-6249; ASTM D-149
Fujipoly Industries Sarcon® GR-d Gap Filler Pad
Sarcon GR-d is a highly conformable, thermally conductive material in areas where space between surfaces is uneven and surface textures vary.Information provided by Fujipoly Industries
Dielectric Breakdown 14000 V
14000 V
0.25 inch electrodes in dry air @25°C; ASTM D149-81
DuPont Teijin Films Melinex® S Polyester Film, 400 Gauge
Melinex® S is a general purpose film which combines excellent handling characteristics with a slightly hazy appearance. It is available in specific thicknesses from 48 - 500 gauge, and is used for ..