Polymer Property : Dielectric Breakdown = 13000 V Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Breakdown 13000 V
13000 V
Withstand Voltage [V/min]; JIS-K-6249; ASTM D-149
Fujipoly Industries Sarcon® GR-Hm Gap Filler Pad
Sarcon GR-m is a highly formable, thermally conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and ..
Dielectric Breakdown 13000 V
13000 V
Withstand Voltage [V/min]; JIS-K-6249; ASTM D-149
Fujipoly Industries Sarcon® GR-m Gap Filler Pad
Sarcon GR-m is a highly formable, thermally conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and ..
Dielectric Breakdown 13000 V
13000 V
Withstand Voltage [V/min]; JIS-K-6249; ASTM D-149
Fujipoly Industries Sarcon® GR-Hd Gap Filler Pad
Sarcon GR-d is a highly conformable, thermally conductive material in areas where space between surfaces is uneven and surface textures vary. GR-Hd has a hardened top surface.Information provided by..
Dielectric Breakdown 13000 V
13000 V
Saint-Gobain CHR® 2045-5 Skived PTFE Film Backing Silicone Adhesive Pressure Sensitive Tape
Description: PTFE films provide a conformable release surface and exhibit a remarkably low coefficient of friction and non-stick properties. PTFE films have high temperature resistance and are virtu..
Dielectric Breakdown 13000 V
13000 V
Saint-Gobain CHR® TV Skived PTFE Film Backing Silicone Adhesive Pressure Sensitive Tape
Description: PTFE films provide a conformable release surface and exhibit a remarkably low coefficient of friction and non-stick properties. PTFE films have high temperature resistance and are virtu..