Electrical Properties | Metric | English | Comments |
---|---|---|---|
Exciting Power (RMS) | 3.1693 RMS AT/cm @Magnetic Field 1.90 T, Frequency 60.0 Hz |
5.0091 RMS VA/lb @Magnetic Field 1.90 T, Frequency 60.0 Hz |
ASTM A804, 0.27 mm |
AK Steel TRAN-COR® H-1 CARLITE® Grain Oriented Electrical Steel TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l.. |