Electrical Properties | Metric | English | Comments |
---|---|---|---|
Exciting Power (RMS) | 0.00261 RMS AT/cm @Magnetic Field 0.100 T, Frequency 50.0 Hz |
0.00413 RMS VA/lb @Magnetic Field 0.100 T, Frequency 50.0 Hz |
Epstein Specimen, 0.009"; ASTM A343 |
AK Steel CARLITE® M-3 Grain Oriented Electrical Steel Oriented Electrical Steels are iron-silicon alloys that were developed to provide the low core loss and high permeability required for efficient and economical electrical transformers. First produce.. |