Electrical Properties | Metric | English | Comments |
---|---|---|---|
Insulation Resistance | 9.40e+12 ohm | 9.40e+12 ohm | 100VDC, 60 sec; Mil-I-46058C |
3M 7995MP Hi-Performance Acrylic 200MP This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia.. |