Electrical Properties Metric English Comments
Insulation Resistance >= 5.00e+6 ohm

@Diameter 8.00 - 10.0 mm
>= 5.00e+6 ohm

@Diameter 0.315 - 0.394 in
After immersion in water; IEC 1212-2 5.2
Hippe PF CC 32 Woven Cotton Cloth Reinforced Phenolic Resin - Round, Molded Tube and Rod
Used in mechanical, electrical and electronic applications. Coarse weave (18 to 30 threads per cm).Information provided by Hippe.
Insulation Resistance >= 5.00e+6 ohm

@Diameter 8.00 - 10.0 mm
>= 5.00e+6 ohm

@Diameter 0.315 - 0.394 in
After immersion in water; IEC 1212-2 5.2
Hippe PF CC 41 Woven Cotton Cloth Reinforced Phenolic Resin - Round, Molded Tube and Rod
Used in mechanical and electrical applications. Fine weave (more than 30 threads per cm).Information provided by Hippe.
Insulation Resistance >= 5.00e+6 ohm

@Diameter 8.00 - 10.0 mm
>= 5.00e+6 ohm

@Diameter 0.315 - 0.394 in
After immersion in water; IEC 1212-2 5.2
Hippe PF CP 23 Cellulose Paper Reinforced Phenolic Resin - Round, Rolled Tube
Used in mechanical and low-voltage electrical applications. Good electrical properties when exposed to normal and high relative humidity.Information provided by Hippe.
Insulation Resistance 5.00e+6 ohm

@Thickness >=3.00 mm
5.00e+6 ohm

@Thickness >=0.118 in
24hr/50°C+24h in water at 23°C; IEC 60167; IEC/EN 60893-2 6.3
Elektro-Isola Etronit 201 MBM Phenolic/melamine, Paper Reinforcement, Grey/also other Colors, Sheets
Description: This material is not standardized, but the base material is the same as Etronit 201 M. The surfaces consist of melamine, which ensures a scratch-resistant, tracking-resistant surface. T..
Insulation Resistance 5.00e+6 ohm

@Thickness >=3.00 mm
5.00e+6 ohm

@Thickness >=0.118 in
24hr/50°C+24h in water at 23°C; IEC 60167; IEC/EN 60893-2 6.3
Elektro-Isola Etronit 201M Phenolic, Paper Reinforcement, Dark Brown, Sheets
Description: Grade with high mechanical properties but the lowest electrical properties of all Etronit types. Used for mechanical applications.Applications: Dies, topplates and back-up plates for dr..
Insulation Resistance 5.00e+6 ohm

@Thickness >=3.00 mm
5.00e+6 ohm

@Thickness >=0.118 in
24hr/50°C+24h in water at 23°C; IEC 60167; IEC/EN 60893-2 6.3
Elektro-Isola Etronit 201M S Phenolic, Paper Reinforcement, Black, Sheets
Description: Grade with high mechanical properties but the lowest electrical properties of all Etronit types. Used for mechanical applications. The material is black throughout. Used where the mecha..