Electrical Properties | Metric | English | Comments |
---|---|---|---|
Insulation Resistance | 3.80e+14 ohm | 3.80e+14 ohm | ASTM D257 |
Unitika UNILATE® 1 NC PET Flame resisting gradeUNILATE® products are plate materials prepared by using a polyethylene terephthalate (PET resin) as the main component, blending it with glass staple fiber, inorganic filler, a.. |