Electrical Properties Metric English Comments
Insulation Resistance 3.05e+10 ohm

@Time 346000 sec
3.05e+10 ohm

@Time 96.0 hour
Control; IPC B25A
Indium Corp. 1075-EX VOC-Free Wave Solder Flux
1075-EX VOC-free, is a resin/rosin-free flux specifically developed for wave soldering, surface mount, mixed technology and through-hole electronic assemblies.1075-EX VOC-Free is a water-based, non-..