Polymer Property : Insulation Resistance = 3.00e+13 ohm
Polymer Property :
Insulation Resistance =
3.00e+13 ohm
Product List
Electrical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties
Metric
English
Comments
Insulation Resistance
3.00e+13
ohm
3.00e+13
ohm
Initial
3M Scotch-Weld™ DP270 Black Structural Adhesive
Rigid potting compound, Non-corrosiveInformation provided by 3M